Skip to content
Industry guide · Automotive & Vehicle Castings

Tie Rod End Housing for Automotive & Transport

For vehicle, commercial-vehicle and rail equipment manufacturers. Specified to IATF 16949, PPAP and the customer's own drawing tolerances.

The Tie Rod End Housing is supplied to vehicle, commercial-vehicle and rail equipment manufacturers as an investment casting, in 5 catalogued sizes by overall length. In this sector the governing consideration is volume, repeatability and a dimensional record that survives a PPAP submission.

Specified to
IATF 16949, PPAP and the customer's own drawing tolerances
Governing factor
Volume, repeatability and a dimensional record that survives a PPAP submission
Failure mode to design out
Process drift that shows up as a capability index falling below the contract minimum
Alloys
WCB, AISI 4140 Cast, AISI 8620 Cast, HK30
Tie Rod End Housing investment castings for Automotive & Transport

Alloys Specified for This Part in Automotive & Transport

Which of these is right depends on the medium, the temperature and the pressure rather than on the sector alone — two plants in the same industry routinely specify different grades for the same part.

GradeSpecificationCorrosionTemperature
WCB ASTM A216 WCB / UNS J03002 None inherent — carbon steel castings are painted, plated or galvanized for corrosion protection. approx. -29 C to +425 C
AISI 4140 Cast ASTM A732 Gr 4140 / UNS G41400 (42CrMo4) None inherent; specify plating or a coating. approx. -40 C to +425 C
AISI 8620 Cast ASTM A732 Gr 8620 / UNS G86200 None inherent; case-hardened surfaces are usually oiled or phosphated. approx. -40 C to +400 C
HK30 ASTM A297 HK30 / UNS J94203 (GX40CrNiSi25-12) Excellent oxidation resistance in hot air and exhaust gas; not a wet-corrosion alloy. continuous service to approx. +1050 C
HK40 ASTM A297 HK40 / UNS J94204 Excellent oxidation resistance; not for wet corrosion. continuous service to approx. +1100 C
A356 / A356-T6 ASTM B26 A356-T6 / AlSi7Mg0.3 Good atmospheric resistance; anodize or coat for marine exposure. approx. -50 C to +150 C
Ti-6Al-4V (Grade 5) ASTM B367 Gr C-5 / UNS R56400 (Ti-6Al-4V) Immune to seawater corrosion; excellent in oxidizing acids, poor in reducing acids and hot chlorides. approx. -253 C to +400 C

Alloys & Grades

The Tie Rod End Housing is cast in 7 of the 63 grades we work in. Those are listed first; the full reference tree is underneath, with each designation shown alongside its ASTM/UNS, EN and GB equivalents.

  • WCB ASTM A216 WCB / UNS J03002
  • AISI 4140 Cast ASTM A732 Gr 4140 / UNS G41400 (42CrMo4)
  • AISI 8620 Cast ASTM A732 Gr 8620 / UNS G86200
  • HK30 ASTM A297 HK30 / UNS J94203 (GX40CrNiSi25-12)
  • HK40 ASTM A297 HK40 / UNS J94204
  • A356 / A356-T6 ASTM B26 A356-T6 / AlSi7Mg0.3
  • Ti-6Al-4V (Grade 5) ASTM B367 Gr C-5 / UNS R56400 (Ti-6Al-4V)
Browse all 63 cast grades we work instainless · carbon & low-alloy · nickel & cobalt · copper · aluminium · titanium
Stainless Steel Castings produced by investment casting

Austenitic Cast Stainless Steel

  • CF8 ASTM A351 CF8 · UNS J92600 · AISI 304 cast · EN 1.4308
  • CF3 ASTM A351 CF3 · UNS J92500 · AISI 304L cast · EN 1.4309
  • CF8M ASTM A351 CF8M · UNS J92900 · AISI 316 cast · EN 1.4408
  • CF3M ASTM A351 CF3M · UNS J92800 · AISI 316L cast · EN 1.4409
  • CF8C ASTM A351 CF8C · UNS J92710 · AISI 347 cast · EN 1.4552
  • CG8M ASTM A351 CG8M · UNS J93000 · AISI 317 cast
  • CN7M ASTM A351 CN7M · UNS N08007 · Alloy 20 cast · Carpenter 20
  • CK3MCuN ASTM A351 CK3MCuN · UNS J93254 · 254 SMO cast · EN 1.4547
  • CN3MN ASTM A351 CN3MN · UNS J94651 · AL-6XN cast

Martensitic Cast Stainless Steel

  • CA15 ASTM A743 CA15 · UNS J91150 · AISI 410 cast · EN 1.4008
  • CA40 ASTM A743 CA40 · UNS J91153 · AISI 420 cast · EN 1.4034
  • CA6NM ASTM A743 CA6NM · UNS J91540 · EN 1.4313 · GX4CrNi13-4
  • CA15M ASTM A743 CA15M · UNS J91151
  • CA6N ASTM A743 CA6N · UNS J91650

Precipitation-Hardening Cast Stainless Steel

  • CB7Cu-1 (17-4 PH) ASTM A747 CB7Cu-1 · UNS J92180 · 17-4 PH cast · AISI 630
  • CB7Cu-2 (15-5 PH) ASTM A747 CB7Cu-2 · UNS J92110 · 15-5 PH cast
Duplex & Super Duplex Cast Stainless Steel investment castings

Duplex & Super Duplex Cast Stainless Steel

  • CD3MN (2205) ASTM A890 Gr 4A · UNS J92205 · Duplex 2205 cast · EN 1.4470
  • CE3MN (2507) ASTM A890 Gr 5A · UNS J93404 · Super Duplex 2507 cast · EN 1.4469
  • CD4MCu ASTM A890 Gr 1A · UNS J93370
  • CD3MWCuN (Zeron 100) ASTM A890 Gr 6A · UNS J93380 · Zeron 100 cast
Heat-Resistant Cast Stainless Steel investment castings

Heat-Resistant Cast Stainless Steel

  • HK30 ASTM A297 HK30 · UNS J94203 · GX40CrNiSi25-12
  • HK40 ASTM A297 HK40 · UNS J94204 · EN 1.4848
  • HH ASTM A297 HH · UNS J93503 · EN 1.4837 cast
  • HT ASTM A297 HT · UNS J94605
  • HP ASTM A297 HP · UNS J95705 · GX40NiCrSi35-25
Carbon & Low-Alloy Steel Castings produced by investment casting

Carbon Steel Castings

  • WCB ASTM A216 WCB · UNS J03002 · GP240GH · EN 1.0619
  • WCC ASTM A216 WCC · UNS J02503
  • WCA ASTM A216 WCA · UNS J02502
  • LCB ASTM A352 LCB · UNS J03003
  • LCC ASTM A352 LCC · UNS J02505
  • AISI 1045 Cast ASTM A732 Gr 1045 · UNS G10450 · C45 · 45#
Low-Alloy Steel Castings investment castings

Low-Alloy Steel Castings

  • AISI 4140 Cast ASTM A732 Gr 4140 · UNS G41400 · 42CrMo4 · EN 1.7225
  • AISI 8620 Cast ASTM A732 Gr 8620 · UNS G86200 · 20CrNiMo
  • WC6 ASTM A217 WC6 · UNS J12072 · 1.25Cr-0.5Mo · G17CrMo5-5
  • WC9 ASTM A217 WC9 · UNS J21890 · 2.25Cr-1Mo · G17CrMo9-10
  • C5 ASTM A217 C5 · UNS J42045 · 5Cr-0.5Mo
  • C12A ASTM A217 C12A · UNS J84090 · Grade 91 · 9Cr-1Mo-V
  • AISI 4340 Cast ASTM A732 Gr 4340 · UNS G43400 · 40CrNiMoA

Nickel-Base Alloy Castings

  • Inconel 625 (CW6MC) ASTM A494 CW6MC · UNS N26625 · Inconel 625 · Alloy 625
  • Inconel 718 AMS 5383 · UNS N07718 · Alloy 718 · GH4169
  • Inconel 713C AMS 5391 · UNS N07713 · Alloy 713C
  • Hastelloy C (CW6M) ASTM A494 CW6M · UNS N30107 · Hastelloy C cast
  • Hastelloy C-276 (CW12MW) ASTM A494 CW12MW · UNS N30002 · Alloy C-276 cast
  • Monel M-35-1 ASTM A494 M35-1 · UNS N24135 · Monel 400 cast

Cobalt-Base Alloy Castings

  • CoCrMo (ASTM F75) ASTM F75 · UNS R30075 · CoCr28Mo6
  • Stellite 6 UNS R30006 · CoCr-A · Alloy 6
  • Stellite 12 UNS R30012 · Alloy 12
  • X-40 (Co-Cr-W) AMS 5382 · UNS R30031 · Haynes 31
Copper Alloy Castings produced by investment casting

Bronze Castings

  • C95800 Nickel Aluminum Bronze ASTM B148 C95800 · UNS C95800 · NAB · CuAl10Fe5Ni5
  • C95500 Nickel Aluminum Bronze ASTM B148 C95500 · UNS C95500
  • C90300 Tin Bronze ASTM B584 C90300 · UNS C90300 · 88-8-0-4
  • C93200 Bearing Bronze ASTM B584 C93200 · UNS C93200 · SAE 660

Brass Castings

  • C83600 Red Brass ASTM B584 C83600 · UNS C83600 · 85-5-5-5
  • C87600 Silicon Brass ASTM B584 C87600 · UNS C87600
  • C86300 Manganese Bronze ASTM B584 C86300 · UNS C86300

Aluminum Alloy Castings

  • A356 / A356-T6 ASTM B26 A356 · UNS A13560 · AlSi7Mg0.3 · EN AC-42000
  • A357 ASTM B26 A357 · UNS A13570 · AlSi7Mg0.6
  • 355 / C355 ASTM B26 355 · UNS A03550 · AlSi5Cu1Mg
  • A201-T7 ASTM B26 A201 · UNS A02010 · AlCu4MgTi

Titanium Castings

  • Ti-6Al-4V (Grade 5) ASTM B367 Gr C-5 · UNS R56400 · TC4 · Ti-6-4
  • CP Titanium Grade 2 ASTM B367 Gr C-2 · UNS R50400

Special & Wear Alloys

  • Ni-Resist D-2 ASTM A439 D-2 · UNS F43000
  • High-Chrome White Iron ASTM A532 Class III · 25Cr white iron

Technical Drawing

Every parameter below is editable, and the drawing redraws to match the values you choose. Picking a size snaps the other fields to that size's values; you can then override any one of them.

Sends the selected values to the quote form below.

Request a Quotation

The form follows the drawing configuration above. Attaching a drawing or a STEP file is the fastest route to a firm price.

Request a Quotation

Specification
Business Information

Dimensions & Parameters

Nominal casting dimensions before machining allowance. Every row is a starting point for the customizer above.

SizeOverall Length L (mm)Overall Width W (mm)Overall Height H (mm)Main Thickness T (mm)Hole Diameter ØD (mm)Min. Wall Thickness (mm)Fillet Radius R (mm)Casting Weight (kg)
60 mm6037.243.28.455.26.50.23
75 mm7546.55410.556.58.50.44
90 mm9055.864.812.657.8100.76
110 mm11068.279.215.479.5101.39
140 mm14086.8100.819.6812.2102.87

Frequently Asked Questions

What matters most for a tie rod end housing in Automotive & Transport?

Volume, repeatability and a dimensional record that survives a PPAP submission. The failure this sector designs out is process drift that shows up as a capability index falling below the contract minimum.

Which specifications apply in Automotive & Transport?

Commonly IATF 16949, PPAP and the customer's own drawing tolerances. Name the one your drawing works to on the RFQ — it changes the testing, the documentation and the price, and it is cheaper to agree before tooling than after.

Which alloys are used for a tie rod end housing in Automotive & Transport?

Commonly WCB, AISI 4140 Cast, AISI 8620 Cast, HK30 and HK40. The right one depends on the medium, the temperature and the pressure rather than on the sector alone — two plants in the same industry routinely specify different grades for the same part.

How do I request a quotation?

Configure the drawing on this page — size, alloy, finish — and submit the form. Attaching a drawing or a STEP file is the fastest route to a firm price, and it lets us flag a castability issue before you commit to tooling.